What is Micralox's Coating Thickness?

Optimal anodized coating thickness for MICRALOX is 1.5 to 2.0 mils. As with all hard coat processes, half of the coating forms below the surface and half grows above the surface, resulting in a larger overall dimension. (.002 coating adds .001 per surface)